詳細(xì)數(shù)據(jù)
訂購(gòu)指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 熔體流動(dòng)速率 | ASTM D-1238 | 0.3 | g/10min | |
密度 | ASTM D-1505 | 0.91 | g/cm3 | ||
機(jī)械性能 | 洛氏硬度 | ASTM D-785 | 80 | R Scale | |
抗張強(qiáng)度(屈服) | ASTM D-638 | 280 | |||
Izod沖擊強(qiáng)度 | 缺口 -20℃ | ASTM D-256 | 10 | ||
Izod沖擊強(qiáng)度 | 無(wú)缺口 23℃ | ASTM D-256 | NB | ||
Izod沖擊強(qiáng)度 | 缺口 23℃ | ASTM D-256 | 90 | ||
Izod沖擊強(qiáng)度 | 缺口 0℃ | ASTM D-256 | 70 | ||
斷裂伸長(zhǎng)率 | ASTM D-638 | >600 | % | ||
彎曲模量 | ASTM D-790 | 13,000 | |||
Izod沖擊強(qiáng)度 | 缺口 -10℃ | ASTM D-256 | 15 | ||
熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 155 | ℃ |