性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 熔體流動速率 | ASTM D-1238 | 9.0 | g/10min | |
吸水率 | ASTM D-570 | 0.22 | % | ||
物理性能 | 比重 | ASTM D-792 | 1.41 | ||
機(jī)械性能 | 洛氏硬度 | ASTM D-785 | 80 | Mscal | |
拉伸長率 | ASTM D-638 | 65 | % | ||
拉伸強(qiáng)度 | ASTM D-638 | 640 | Kg/cm2 | ||
彎曲強(qiáng)度 | ASTM D-790 | 920 | Kg/cm2 | ||
彎曲彈性率 | ASTM D-790 | 26500 | Kg/cm2 | ||
摩擦系數(shù) | ASTM D-1894 | 0.22 | |||
IZOD缺口沖擊強(qiáng)度 | ASTM D-256 | 7.0 | kg.cm/cm | ||
電氣性能 | 表面電阻系數(shù) | ASTM D-257 | 1×1016 | Ω.cm | |
介電損耗正切 | ASTM D-150 | 0.006 | |||
絕緣破壞電壓 | ASTM D-149 | 19 | KV/mm | ||
耐ARC性 | ASTM D-495 | >200 | sec | ||
體積電阻系數(shù) | ASTM D-257 | 1×1014 | Ω | ||
介電常數(shù) | ASTM D-150 | 3.7 | |||
加工性能 | 成型收縮率 | ASTM D-955 | 2.0 | % | |
熱性能 | 熱變形溫度 | 18.6 | ASTM D-648 | 110 | ℃ |
線膨脹系數(shù) | ASTM D-696 | 11-13 | ×10-5cm/cm/℃ | ||
熱變形溫度 | 4.6 | 160 | Kg/cm2 | ||
熔點(diǎn) | ASTM D-1525 | 166 | ℃ | ||
燃燒性 | UL 94 | HB |