詳細(xì)數(shù)據(jù)
訂購(gòu)指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 密度 | ExxonMobil Method | 0.882 | g/cm3 | |
霧度2 | ASTM D-1003 | 13@50mils | % | ||
熔融指數(shù) | ASTM D-1238 | 10.0 | g/10 min | ||
熔體流動(dòng)速率 | ASTM D-1238 | 25 | g/10 min | ||
硬度2 | Shore D,15 sec | ASTM D-2240 | 27 | ||
硬度2 | Shore A,15 sec | ASTM D-2240 | 79 | ||
物理性能 | 拉伸強(qiáng)度3 | @Break | ASTM D-638 | No Break | psi(MPa) |
缺口沖擊強(qiáng)度 | -40℃ | ASTM D-256 | No Break | ft-lb/in(J/m) | |
彎曲模量 | 1% secant | ASTM D-790 | 3807(26.2) | psi(MPa) | |
缺口沖擊強(qiáng)度 | 23℃ | ASTM D-256 | No Break | ft-lb/in(J/m) | |
拉伸率 | @Break | ASTM D-638 | No Break | % | |
熱性能 | 最高熔體溫度 | ExxonMobil Method | 164.7(73.7) | ℉(℃) | |
維卡軟化點(diǎn)2 | 200g | ASTM D-1525 | 159.8(71.0) | ℉(℃) | |
其它性能 | 拉伸應(yīng)力5 | @100% Elongation | ASTM D-412 | 407(2.8) | psi(MPa) |
拉伸應(yīng)力5 | @300% Elongation | ASTM D-412 | 493(3.4) | psi(MPa) | |
門尼粘度ML(1+4) | 125℃ | ASTM D-1646 | 5.9 | Torgue Units | |
抗扯強(qiáng)度 | ASTM D-624 | 245.9(43.1) | lb/in(kN/m) | ||
拉伸率 | @Break | ASTM D-412 | No Break | % |