密度 | 1.18g/cm3 | 熔體流動速率 | 1g/10min | 吸水率 | 0.3% |
缺口沖擊強(qiáng)度 | 1.6 | 成型收縮率 | 0.4% | 特性級別 | 透明級 |
|
產(chǎn)品簡述
密度 | 1.18g/cm3 | 熔體流動速率 | 1g/10min | 吸水率 | 0.3% |
缺口沖擊強(qiáng)度 | 1.6 | 成型收縮率 | 0.4% | 特性級別 | 透明級 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 吸水率 | 24h | ASTM D-570 | 0.3 | % |
物理性能 | 反射指數(shù) | ASTM D-542 | 1.49 | ||
透明性 | 3.2mm | ASTM D-1003 | 93 | % | |
比重 | ASTM D-792 | 1.18 | |||
機(jī)械性能 | 洛氏硬度 | M-Scale | ASTM D-785 | 97 | |
沖擊強(qiáng)度 | Izod Notched | ASTM D-256 | 1.6 | kg·cm/cm2 | |
彎曲模數(shù) | ASTM D-790 | 33,000 | Kg/cm2 | ||
拉力 | ASTM D-638 | 740 | Kg/cm2 | ||
延伸率 | ASTM D-638 | 3.5 | % | ||
??s系數(shù) | ASTM D995-51 | 0.2-0.6 | % | ||
彎曲強(qiáng)度 | ASTM D-790 | 1,330 | Kg/cm2 | ||
電氣性能 | 介電強(qiáng)度 | 4KV/S | ASTM D-149 | 20 | KV/mm |
介電定數(shù) | 60Hz | ASTM D-150 | 4 | ||
功率系數(shù) | 60Hz | ASTM D-150 | 0.05 | ||
抗體積系數(shù) | ASTM D-257 | >1515 | Ω.m | ||
熱性能 | 熱傳導(dǎo) | ASTM D-177 | 5×10-4 | cal/seccm·°C/cm | |
綿性膨脹系數(shù) | ASTM D-696 | 6×10-5 | cm/cm/°C | ||
維卡軟化點(diǎn) | 1kg | ASTM D-1525 | 105 | °C | |
比熱 | 0.35 | cal/g/°C | |||
熱變形溫度 | 18.56kg | ASTM D-648 | 98 | °C | |
燃燒度 | UL94 | HB | 1/8",1/16" | ||
流動指數(shù) | 230°C,3.8kg | ASTM D-1238 | 1.0 | g/10min |