用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜吹塑 | 加工級別 | 吹塑級 |
|
產(chǎn)品簡述
用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜吹塑 | 加工級別 | 吹塑級 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 密度 | ASTM D1505 | 0.922 | g/cm3; | |
熔流率 | 190℃/2.16 kg | ASTM D1238 | 2.0 | g/10 min | |
機(jī)械性能 | 摩擦系數(shù) | 吹塑薄膜 | ASTM D1894 | 0.050 | |
薄膜厚度 - 經(jīng)測試 | 30 | µm | |||
抗張強(qiáng)度 | MD: 斷裂, 30 µm, 吹塑薄膜 | ASTM D882 | 40.0 | MPa | |
TD: 斷裂, 30 µm, 吹塑薄膜 | ASTM D882 | 20.0 | MPa | ||
伸長率 | MD: 斷裂, 30 µm, 吹塑薄膜 | ASTM D882 | 700 | % | |
TD: 斷裂, 30 µm, 吹塑薄膜 | ASTM D882 | 850 | % | ||
落錘沖擊 | 30 µm, 吹塑薄膜 | ASTM D1709 | 70 | g | |
Elmendorf Tear Strength | MD: 30.0 µm, Blown Film | ASTM D1922 | 29.4 | kN/m | |
TD: 30.0 µm, Blown Film | ASTM D1922 | 147.1 | kN/m | ||
熱性能 | 脆化溫度 | ASTM D746 | < -70.0 | ℃ | |
維卡軟化溫度 | ASTM D1525 | 101 | ℃ | ||
光性能 | 光澤度 | 45°,30 µm, 吹塑薄膜 | ASTM D2457 | 46 | |
透明度 | 30 µm, 吹塑薄膜 | ASTM D1746 | 25.0 | ||
霧度 | 30 µm, 吹塑薄膜 | ASTM D1003 | 20 | % |