性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 密度 | ASTM D-792 | 0.927 | g/cm3 | |
熔體流動(dòng)速率 | 190℃/2.16 kg | ASTM D-1238 | 4.5 | g/10min | |
厚度 | 50.8 | microns | |||
水汽傳輸 | ASTM F-372 | 4.3 | |||
機(jī)械性能 | 拉伸屈服強(qiáng)度 | MD | ASTM D-882 | 11.8 | MPa |
拉伸屈服強(qiáng)度 | TD | ASTM D-882 | 13.8 | MPa | |
埃爾曼多夫撕裂強(qiáng)度 | MD | ASTM D-1922 | 69 | g | |
埃爾曼多夫撕裂強(qiáng)度 | TD | ASTM D-1922 | 241 | g | |
斷裂伸長率 | MD | ASTM D-882 | 780 | % | |
斷裂伸長率 | TD | ASTM D-882 | 840 | % | |
屈服伸長率 | MD | ASTM D-882 | 12 | % | |
屈服伸長率 | TD | ASTM D-882 | 9 | % | |
拉伸斷裂強(qiáng)度 | MD | ASTM D-882 | 22.9 | MPa | |
拉伸斷裂強(qiáng)度 | TD | ASTM D-882 | 2.1 | MPa | |
熱性能 | 維卡軟化點(diǎn) | ASTM D-1003 | 103 | ℃ | |
熔融溫度 | 210 | ℃ | |||
爆破比(BUR) | 2 |