性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
基本性能 | 密度 | ASTM D-792 | 0.921 | g/cm3 | |
熔體流動(dòng)速率 | ASTM D-1238 | 0.5 | g/10min | ||
厚度 | 30.5 | microns | |||
機(jī)械性能 | 落錘 | ASTM D-1709 | 8.54 | g/micron | |
拉伸屈服強(qiáng)度 | ASTM D-882 | 11 | MPa | ||
拉伸屈服強(qiáng)度 | ASTM D-882 | 11.9 | MPa | ||
割線模量 | ASTM D-882 | 0.272 | GPa | ||
割線模量 | ASTM D-882 | 0.317 | GPa | ||
斷裂伸長率 | MD | ASTM D-882 | 590 | % | |
斷裂伸長率 | TD | ASTM D-882 | 730 | % | |
埃爾曼多夫撕裂強(qiáng)度 | MD | ASTM D-1922 | 340 | g | |
埃爾曼多夫撕裂強(qiáng)度 | TD | ASTM D-1922 | 760 | g | |
拉伸斷裂強(qiáng)度 | MD | ASTM D-882 | 63.9 | MPa | |
拉伸斷裂強(qiáng)度 | TD | ASTM D-882 | 55.4 | MPa | |
埃爾曼多夫撕裂強(qiáng)度 | MD | ASTM D-1922 | 11.1 | g/micron | |
埃爾曼多夫撕裂強(qiáng)度 | TD | ASTM D-1922 | 24.9 | g/micron | |
熱性能 | 熔點(diǎn) | 125 | ℃ | ||
光學(xué)性能 | 霧度 | ASTM D-1003 | 10 | % | |
光澤度 | ASTM D-2457 | 54 | % |