性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 密度 | ASTM D-792 | 0.932 | g/cm3 | |
熔體流動速率 | 190℃/2.16 kg | ASTM D-1238 | 0.5 | g/10min | |
厚度 | 20.3 | microns | |||
粘連性 | 3500 | ppm | |||
爽滑性 | 1200 | ppm | |||
機械性能 | 拉伸屈服強度 | MD | ASTM D-882 | 25.1 | MPa |
拉伸屈服強度 | TD | ASTM D-882 | 25.8 | MPa | |
斷裂伸長率 | MD | ASTM D-882 | 530 | % | |
斷裂伸長率 | TD | ASTM D-882 | 716 | % | |
沖擊強度 | TD | ASTM D-882 | 4414 | ||
沖擊強度 | MD | ASTM D-882 | 5723 | ||
割線模量 | MD,2% | ASTM D-882 | 0.299805 | GPa | |
割線模量 | TD,2% | ASTM D-882 | 0.315559 | GPa | |
埃爾曼多夫撕裂強度 | MD | ASTM D-1922 | 332 | g | |
埃爾曼多夫撕裂強度 | TD | ASTM D-1922 | 599 | g | |
埃爾曼多夫撕裂強度 | MD | ASTM D-1922 | 16.3 | g/micron | |
埃爾曼多夫撕裂強度 | TD | ASTM D-1922 | 29.5 | g/micron | |
落錘沖擊 | Method B | ASTM D-1709 | Max100 | g | |
落錘沖擊 | Method A | ASTM D-1709 | 126 | g | |
拉伸斷裂強度 | MD | ASTM D-882 | 78.4 | MPa | |
拉伸斷裂強度 | TD | ASTM D-882 | 75.5 | MPa | |
熱封強度 | Dow Method | 12.9 | N | ||
熱性能 | 熱封強度始封溫度 | Dow Method | 120 | ℃ | |
熔點 | 126 | ℃ | |||
維卡軟化點 | 119 | ℃ | |||
光學性能 | 霧度 | 13 | % | ||
光澤度 | 20 ° | 46 | % | ||
光澤度 | 45 ° | 49 | % |