斷裂伸長率 | 800% | 拉伸強度 | 33MPa | 密度 | 0.919g/cm3 |
熔體流動速率 | 2g/10min | 維卡軟化點 | 102℃ | 用途級別 | 薄膜級,電線電纜級 |
規(guī)格級別 | 高光澤薄膜吹塑 | 加工級別 | 吹塑級 | 特性級別 | 高光澤 |
|
產品簡述
斷裂伸長率 | 800% | 拉伸強度 | 33MPa | 密度 | 0.919g/cm3 |
熔體流動速率 | 2g/10min | 維卡軟化點 | 102℃ | 用途級別 | 薄膜級,電線電纜級 |
規(guī)格級別 | 高光澤薄膜吹塑 | 加工級別 | 吹塑級 | 特性級別 | 高光澤 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.919 | g/cm3 | ||
物理性能 | 熔體流動速率 | ASTM D-1238 | 2.0 | g/10min | ||
薄膜厚度 | 25 | μm | ||||
機械性能 | 抗張強度(屈服點) | MD | ASTM D-882 | 120 | Kg/cm2 | |
TD | ASTM D-882 | 110 | Kg/cm2 | |||
斷裂伸長率 | MD | ASTM D-882 | 650 | % | ||
TD | ASTM D-882 | 800 | % | |||
抗張強度(斷裂點) | MD | ASTM D-882 | 380 | Kg/cm2 | ||
TM | ASTM D-882 | 340 | Kg/cm2 | |||
抗張模數(shù) | MD | ASTM D-882 | 2000 | Kg/cm2 | ||
TD | ASTM D-882 | 2500 | Kg/cm2 | |||
撕裂強度 | MD | ASTM D-1004 | 125 | Kg/cm | ||
TD | ASTM D-1004 | 105 | Kg/cm | |||
尖頭沖擊強度 | ASTM D-1709 | 3.7 | g/μm | |||
熱性能 | 低溫脆化溫度 | ASTM D-746 | <-70 | ℃ | ||
軟化點 | ASTM D-1525 | 102 | ℃ |