斷裂伸長率 | 850% | 拉伸強度 | 35MPa | 密度 | 0.919g/cm3 |
熔體流動速率 | 1g/10min | 用途級別 | 薄膜級,纖維 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 10 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
|
產(chǎn)品簡述
斷裂伸長率 | 850% | 拉伸強度 | 35MPa | 密度 | 0.919g/cm3 |
熔體流動速率 | 1g/10min | 用途級別 | 薄膜級,纖維 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 10 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.919 | g/cm3 | ||
熔體流動速率 | ASTM D-1238 | 1 | g/10min | |||
機械性能 | 伸長率 | MD | ASTM D-882 | 750 | % | |
TD | ASTM D-882 | 850 | % | |||
拉伸斷裂強度 | MD | ASTM D-882 | 430 | Kg/cm2 | ||
TD | ASTM D-882 | 360 | Kg/cm2 | |||
拉伸屈服強度 | MD | ASTM D-882 | 120 | Kg/cm2 | ||
TD | ASTM D-882 | 110 | Kg/cm2 | |||
抗沖擊強度 | ASTM D-3420 | 10 | Kg/cm | |||
撕裂強度 | MD | ASTM D-1922 | 5 | g/µm | ||
TD | ASTM D-1922 | 12 | g/µm | |||
熱性能 | 脆化溫度 | ASTM D-746 | <-70 | ℃ | ||
維卡軟化點 | ASTM D-1525 | 102 | ℃ | |||
其它性能 | 霧度 | ASTM D-1003 | 20 | % | ||
薄膜厚度 | ASTM D-746 | 50 | µm |