斷裂伸長率 | 800% | 拉伸強(qiáng)度 | 34MPa | 密度 | 0.918g/cm3 |
熔體流動速率 | 2.1g/10min | 維卡軟化點(diǎn) | 98℃ | 用途級別 | 薄膜級,纖維 |
規(guī)格級別 | 薄膜 | 加工級別 | 注塑級 | 特性級別 | 增強(qiáng)級 |
|
產(chǎn)品簡述
斷裂伸長率 | 800% | 拉伸強(qiáng)度 | 34MPa | 密度 | 0.918g/cm3 |
熔體流動速率 | 2.1g/10min | 維卡軟化點(diǎn) | 98℃ | 用途級別 | 薄膜級,纖維 |
規(guī)格級別 | 薄膜 | 加工級別 | 注塑級 | 特性級別 | 增強(qiáng)級 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 熔體流動速率 | ASTM D-1238 | 2.1 | g/10min | ||
密度 | ASTM D-1505 | 0.918 | g/cm3 | |||
物理性能 | 薄膜厚度 | 25 | µm | |||
機(jī)械性能 | 拉伸斷裂強(qiáng)度 | MD | ASTM D-882 | 400 | Kg/cm2 | |
TD | ASTM D-882 | 350 | Kg/cm2 | |||
撕裂強(qiáng)度 | MD | ASTM D-1004 | 120 | Kg/cm | ||
TD | ASTM D-1004 | 110 | Kg/cm | |||
抗張模數(shù) | MD | ASTM D-882 | 2200 | Kg/cm2 | ||
TD | ASTM D-882 | 3100 | Kg/cm2 | |||
拉伸屈服強(qiáng)度 | MD | ASTM D-882 | 140 | Kg/cm2 | ||
TD | ASTM D-882 | 130 | Kg/cm2 | |||
尖頭沖擊強(qiáng)度 | ASTM D-1709 | 4.0 | g/μm | |||
斷裂伸長率 | MD | ASTM D-882 | 650 | % | ||
TD | ASTM D-882 | 800 | % | |||
熱性能 | 維卡軟化點(diǎn) | ASTM D-1525 | 98 | ℃ | ||
低溫脆化溫度 | ASTM D-746 | <-80 | ℃ |