| 斷裂伸長率 | 800% | 拉伸強(qiáng)度 | 32MPa | 密度 | 0.918g/cm3 |
| 熔體流動(dòng)速率 | 2.1g/10min | 維卡軟化點(diǎn) | 98℃ | 用途級別 | 薄膜級,食品級 |
| 規(guī)格級別 | 薄膜 | 加工級別 | 吹膜級 | 特性級別 | 透明級 |
|
|
產(chǎn)品簡述
| 斷裂伸長率 | 800% | 拉伸強(qiáng)度 | 32MPa | 密度 | 0.918g/cm3 |
| 熔體流動(dòng)速率 | 2.1g/10min | 維卡軟化點(diǎn) | 98℃ | 用途級別 | 薄膜級,食品級 |
| 規(guī)格級別 | 薄膜 | 加工級別 | 吹膜級 | 特性級別 | 透明級 |
詳細(xì)數(shù)據(jù)
訂購指南
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
| 基本性能 | 熔體流動(dòng)速率 | ASTM D-1238 | 2.1 | g/10min | ||
| 密度 | ASTM D-1505 | 0.918 | g/10min | |||
| 物理性能 | 薄膜厚度 | 25 | μm | |||
| 機(jī)械性能 | 斷裂拉伸強(qiáng)度 | MD | ASTM D-882 | 380 | Kg/cm2 | |
| TD | ASTM D-882 | 330 | Kg/cm2 | |||
| 屈服拉伸強(qiáng)度 | MD | ASTM D-882 | 140 | Kg/cm2 | ||
| TD | ASTM D-882 | 130 | Kg/cm2 | |||
| 尖頭沖擊強(qiáng)度 | ASTM D-1709 | 3.5 | g/μm | |||
| 斷裂伸長率 | MD | ASTM D-882 | 650 | % | ||
| TD | ASTM D-882 | 800 | % | |||
| 抗張模數(shù) | MD | ASTM D-882 | 2200 | Kg/cm2 | ||
| TD | ASTM D-882 | 3100 | Kg/cm2 | |||
| 撕裂強(qiáng)度 | MD | ASTM D-1004 | 115 | kg/cm | ||
| TD | ASTM D-1004 | 105 | kg/cm | |||
| 熱性能 | 低溫脆化溫度 | ASTM D-746 | <-75 | ℃ | ||
| 維卡軟化點(diǎn) | ASTM D-1525 | 98 | ℃ | |||