斷裂伸長率 | 855% | 拉伸強度 | 36MPa | 密度 | 0.924g/cm3 |
熔體流動速率 | 1g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 9 |
|
產(chǎn)品簡述
斷裂伸長率 | 855% | 拉伸強度 | 36MPa | 密度 | 0.924g/cm3 |
熔體流動速率 | 1g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 9 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 薄膜厚度 | ASTM D-746 | 50 | μm | ||
熔融指數(shù) | ASTM D-1238 | 1.0 | g/10min | |||
密度 | ASTM D-1505 | 0.924 | g/cm3 | |||
機械性能 | 撕裂強度 | MD | ASTM D-1992 | 4 | g/μm | |
TD | ASTM D-1992 | 11 | g/μm | |||
拉伸強度 | (斷裂點)MD | ASTM D-882 | 453 | kg/cm2 | ||
(斷裂點)TD | ASTM D-882 | 370 | kg/cm2 | |||
拉伸強度 | (屈服點)MD | ASTM D-882 | 135 | kg/cm2 | ||
(屈服點)TD | ASTM D-882 | 120 | kg/cm2 | |||
抗沖擊強度 | Spencer | ASTM D-3420 | 9 | kg.cm | ||
伸長率 | MD | ASTM D-882 | 765 | % | ||
TD | ASTM D-882 | 855 | % | |||
熱性能 | 脆化溫度 | ASTM D-746 | <-70 | ℃ | ||
維卡軟化點 | ASTM D-1525 | 102 | ℃ | |||
其它性能 | 添加劑 | SK Method | A/B | |||
霧度 | ASTM D-1003 | 22 | % |