斷裂伸長率 | 600% | 拉伸強度 | 20MPa | 密度 | 0.923g/cm3 |
熔體流動速率 | 2.4g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 110 | 加工級別 | 發(fā)泡級 |
|
產(chǎn)品簡述
斷裂伸長率 | 600% | 拉伸強度 | 20MPa | 密度 | 0.923g/cm3 |
熔體流動速率 | 2.4g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 110 | 加工級別 | 發(fā)泡級 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | 23℃ | ASTM D-1505 | 0.923 | g/cm3 | |
熔體流動速率 | ASTM D-1238 | 2.4 | g/10min | |||
機械性能 | 斷裂伸長率 | MD | ASTM D-882 | 550 | % | |
TD | ASTM D-882 | 600 | % | |||
抗沖擊強度 | ASTM D-1709 | 110 | g | |||
斷裂拉伸強度 | MD | ASTM D-882 | 22 | MPa | ||
TD | ASTM D-882 | 20 | MPa | |||
拉伸屈服強度 | MD | ASTM D-882 | 12 | MPa | ||
TD | ASTM D-882 | 11 | MPa | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 94 | ℃ | ||
晶體熔點 | ASTM E-794 | 111 | ℃ | |||
其它性能 | 推薦薄膜厚度 | 25-100 | µm | |||
摩擦系數(shù) | ASTM D-1894 | 0.10 | ||||
光澤度 | ASTM D-2457 | 70 | gu | |||
霧度(濁度) | ASTM D-1003 | 6.5 | % | |||
透明度 | ASTM D-1746 | 85 | % |