斷裂伸長率 | 480% | 拉伸強度 | 11MPa | 密度 | 0.923g/cm3 |
熔體流動速率 | 2g/10min | 用途級別 | 薄膜級,纖維 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 150 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
|
產品簡述
斷裂伸長率 | 480% | 拉伸強度 | 11MPa | 密度 | 0.923g/cm3 |
熔體流動速率 | 2g/10min | 用途級別 | 薄膜級,纖維 | 規(guī)格級別 | 薄膜 |
缺口沖擊強度 | 150 | 加工級別 | 注塑級 | 特性級別 | 增強級 |
詳細數(shù)據
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據 | 數(shù)據單位 | ||
基本性能 | 密度 | 23°C | ASTM D-1505 | 0.923 | g/cm3 | |
熔體流動速率 | ASTM D-1238 | 2.0 | g/10min | |||
機械性能 | 斷裂伸長率 | ASTM D-638 | 480 | % | ||
抗張強度 | ASTM D-638 | 130 | Kg/cm2 | |||
抗撕裂張度 | MD | ASTM D-1922 | 290 | g | ||
TD | ASTM D-1922 | 320 | g | |||
破裂點張力 | MD | ASTM D-882 | 210 | kg/cm2 | ||
TD | ASTM D-882 | 190 | kg/cm2 | |||
跌落沖擊強度 | ASTM D-1709 | 150 | g | |||
屈服點張力 | ASTM D-638 | 115 | Kg/cm2 | |||
斷裂點伸張率 | MD | ASTM D-882 | 550 | % | ||
TD | ASTM D-882 | 650 | % | |||
熱性能 | 低溫脆化溫度 | ASTM D-746 | <-76 | °C | ||
維卡軟化點 | ASTM D-1525 | 97 | °C |