斷裂伸長率 | 600% | 拉伸強度 | 10MPa | 密度 | 0.923g/cm3 |
熔體流動速率 | 2.5g/10min | 用途級別 | 薄膜級,纖維 | 規(guī)格級別 | 薄膜 |
脆化溫度 | -68℃ | 加工級別 | 注塑級 | 特性級別 | 增強級,耐高溫 |
|
產(chǎn)品簡述
斷裂伸長率 | 600% | 拉伸強度 | 10MPa | 密度 | 0.923g/cm3 |
熔體流動速率 | 2.5g/10min | 用途級別 | 薄膜級,纖維 | 規(guī)格級別 | 薄膜 |
脆化溫度 | -68℃ | 加工級別 | 注塑級 | 特性級別 | 增強級,耐高溫 |
詳細數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 熔體流動速率 | 190℃/2.16kg | ASTM D-1238 | 2.5 | g/10min | |
密度 | ASTM D-792 | 0.923 | g/cm3 | |||
機械性能 | 屈服拉伸強度 | MD | ASTM D-882 | 10 | MPa | |
TD | ASTM D-882 | 10 | MPa | |||
最終強度 | MD | ASTM D-882 | 23 | MPa | ||
TD | ASTM D-882 | 17 | MPa | |||
斷裂伸長率 | MD | ASTM D-882 | 350 | % | ||
TD | ASTM D-882 | 600 | % | |||
沖擊強度 | ASTM D-1709 | 1.20 | gf/μm | |||
埃爾曼多夫撕裂強度 | MD | ASTM D-1922 | 4 | gf/μm | ||
TD | ASTM D-1922 | 15 | gf/μm | |||
熱性能 | 脆化溫度 | ASTM D-746 | -68 | ℃ | ||
其它性能 | 透明度 | ASTM D-1003 | 7 | % | ||
光學性能 | 光澤度 | ASTM D-2457 | 42 | % |