斷裂伸長率 | 530% | 拉伸強(qiáng)度 | 16MPa | 密度 | 0.925g/cm3 |
熔體流動速率 | 6.4g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強(qiáng)度 | 36 |
|
產(chǎn)品簡述
斷裂伸長率 | 530% | 拉伸強(qiáng)度 | 16MPa | 密度 | 0.925g/cm3 |
熔體流動速率 | 6.4g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強(qiáng)度 | 36 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-792 | 0.925 | g/cm3 | ||
熔體流動速率 | ASTM D-1338 | 6.4 | g/10min | |||
薄膜厚度 | 25.4 | μ | ||||
機(jī)械性能 | 屈服拉伸強(qiáng)度 | MD | ASTM D-882 | 13.9 | MPa | |
TD | ASTM D-882 | 12.8 | MPa | |||
斷裂拉伸強(qiáng)度 | MD | ASTM D-882 | 25.1 | MPa | ||
TD | ASTM D-882 | 16.0 | MPa | |||
斷裂伸長率 | MD | ASTM D-882 | 340 | % | ||
TD | ASTM D-882 | 530 | % | |||
落鏢沖擊強(qiáng)度 | ASTM D-1709 | 36 | g | |||
埃爾曼多夫撕裂強(qiáng)度 | MD | ASTM D-1922 | 210 | g | ||
TD | ASTM D-1922 | 180 | g | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 96.1 | ℃ | ||
熔點 | DSC | 113 | ℃ | |||
其它性能 | 薄膜韌性 | MD | ASTM D-882 | 141 | J/cm3 | |
TD | ASTM D-882 | 132 | J/cm3 | |||
光學(xué)性能 | 光澤度 | 45° | ASTM D-2457 | 87 | ||
霧度 | ASTM D-1003 | 3.5 | % |