斷裂伸長率 | 680% | 拉伸強(qiáng)度 | 28.4MPa | 密度 | 0.92g/cm3 |
熔體流動速率 | 0.7g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強(qiáng)度 | 150 |
|
產(chǎn)品簡述
斷裂伸長率 | 680% | 拉伸強(qiáng)度 | 28.4MPa | 密度 | 0.92g/cm3 |
熔體流動速率 | 0.7g/10min | 用途級別 | 薄膜級 | 規(guī)格級別 | 薄膜 |
缺口沖擊強(qiáng)度 | 150 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-792 | 0.920 | g/cm3 | ||
熔體流動速率 | ASTM D-1238 | 0.70 | g/10min | |||
薄膜厚度 | 50.8 | μ | ||||
機(jī)械性能 | 屈服拉伸強(qiáng)度 | MD | ASTM D-882 | 12.6 | MPa | |
TD | ASTM D-882 | 11.4 | MPa | |||
斷裂拉伸強(qiáng)度 | MD | ASTM D-882 | 29.7 | MPa | ||
TD | ASTM D-882 | 28.4 | MPa | |||
斷裂伸長率 | MD | ASTM D-882 | 480 | % | ||
TD | ASTM D-882 | 680 | % | |||
落鏢沖擊強(qiáng)度 | ASTM D-1709 | 150 | g | |||
埃爾曼多夫撕裂強(qiáng)度 | MD | ASTM D-1922 | 280 | g | ||
TD | ASTM D-1922 | 350 | g | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 97.8 | ℃ | ||
熔點 | DSC | 112 | ℃ | |||
其它性能 | 薄膜韌性 | MD | ASTM D-882 | 197 | J/cm3 | |
TD | ASTM D-882 | 211 | J/cm3 | |||
光學(xué)性能 | 光澤度 | 45° | ASTM D-2457 | 70 | ||
霧度 | ASTM D-1003 | 8.6 | % |