斷裂伸長率 | 550% | 拉伸強(qiáng)度 | 16MPa | 密度 | 0.918g/cm3 |
熔體流動(dòng)速率 | 2.5g/10min | 缺口沖擊強(qiáng)度 | 100 | 加工級別 | 注塑級 |
|
產(chǎn)品簡述
斷裂伸長率 | 550% | 拉伸強(qiáng)度 | 16MPa | 密度 | 0.918g/cm3 |
熔體流動(dòng)速率 | 2.5g/10min | 缺口沖擊強(qiáng)度 | 100 | 加工級別 | 注塑級 |
詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.918 | g/cm3 | ||
熔體流動(dòng)速率 | MI2.16 | ASTM D-1238 | 2.5 | ℃ | ||
物理性能 | 光澤度 | 45℃ | ASTM D-2457 | 60 | % | |
膜厚度 | 25-80 | μ | ||||
摩擦系數(shù) | ASTM D-1894 | <0.13 | ||||
機(jī)械性能 | 拉力斷裂伸長率 | MD | ASTM D-882B | 250 | % | |
TD | ASTM D-882B | 550 | % | |||
彎曲模量 | ASTM D-790 | 1700 | kg/cm2 | |||
拉力斷裂強(qiáng)度 | MD | ASTM D-882B | 210 | KG/cm2 | ||
TD | ASTM D-882B | 170 | KG/cm2 | |||
抗撕裂性 | MD | ASTM D-1922 | 70 | N/mm | ||
TD | ASTM D-1922 | 50 | N/mm | |||
落球沖擊強(qiáng)度 | ASTM D-1709 | 100 | g | |||
拉力降伏強(qiáng)度 | MD | ASTM D-882B | 100 | KG/cm2 | ||
TD | ASTM D-882B | 110 | KG/cm2 | |||
拉力斷裂強(qiáng)度 | ASTM D-638 | 150 | kg/cm2 | |||
硬度 | ASTM D-2240 | 52 | Shore D | |||
拉力降伏強(qiáng)度 | ASTM D-638 | 100 | kg/cm2 | |||
拉力斷裂伸長率 | ASTM D-638 | 600 | % | |||
1%伸長彈性系數(shù) | MD | ASTM D-882B | 1900 | KG/cm2 | ||
TD | ASTM D-882B | 2200 | KG/cm2 | |||
熱性能 | 脆化溫度 | ASTM D-746 | <-70 | ℃ | ||
熔點(diǎn) | DSC | 107 | ℃ | |||
維卡軟化點(diǎn) | ASTM D-1525 | 95 | ℃ | |||
其它性能 | 濁度 | ASTM D-1003 | 13 | % |