性能項目 | 試驗條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.920 | g/cc | ||
熔體流動速率 | ASTM D-1238 | 3.0 | g/10min | |||
機械性能 | 斷裂拉伸強度 | ASTM D-638 | 165 | kg/cm2 | ||
拉伸抗熱強度 | MD | ASTM D-1004 | 110 | kg/cm | ||
TD | ASTM D-1004 | 105 | kg/cm | |||
下降沖擊強度 | ASTM D-1709 | 200 | g | |||
斷裂拉伸強度 | MD | ASTM D-882 | 280 | kg/cm2 | ||
TD | ASTM D-882 | 250 | kg/cm2 | |||
斷裂伸長率 | ASTM D-638 | 750 | % | |||
斷裂伸長率 | MD | ASTM D-882 | 250 | % | ||
TD | ASTM D-882 | 600 | % | |||
熱性能 | 熔點 | ASTM D-2117 | 110 | ℃ | ||
維卡軟化點 | ASTM D-1525 | 94 | ℃ | |||
其它性能 | 混濁度 | ASTM D1009 | 15.0 | % | ||
厚度 | HCC | 0.06 | ㎜ |