詳細(xì)數(shù)據(jù)
訂購指南
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 | 熔流率 | 190°C/2.16 kg | ASTM D1238 | 1.6 |
g/10 min
|
醋酸乙烯含量 | ExxonMobil Method | 18.5 |
wt%
|
||
機(jī)械性能 | 割線模量 |
1% 正割, MD
|
ASTM D882 | 65.4 |
MPa
|
1% 正割, TD
|
ASTM D882 | 70.5 |
MPa
|
||
抗張強(qiáng)度 |
MD: 斷裂
|
ASTM D882 | 27.2 |
MPa
|
|
TD: 斷裂
|
ASTM D882 | 27.5 |
MPa
|
||
伸長(zhǎng)率 |
MD: 斷裂
|
ASTM D882 | 180 |
%
|
|
TD: 斷裂 | ASTM D882 | 650 |
%
|
||
落錘沖擊 |
|
ASTM D1709A | 370 |
g
|
|
埃爾曼多夫抗撕強(qiáng)度 | MD | ASTM D1922 | 39 |
g
|
|
TD
|
ASTM D1922 | 81 |
g
|
||
熱性能 | 維卡軟化溫度 | ASTM D1525 | 62.0 |
°C
|