Typical Properties | ||
Property | Typical Value, Units | |
Form | Powder | |
Acetyl Content | 1.3 wt % | |
Propionyl Content | 48 wt % | |
Hydroxyl Content | 1.7 wt % | |
Melting Point | 188-210°C | |
Acidity as Acetic Acid | 0.01 wt % | |
Ash Content | 0.017 wt % | |
Refractive Index | 1.475 n(25°C/D) | |
Glass Transition Temperature (Tg) | 147°C | |
Specific Gravity @ 20°C/25°C | 1.22 | |
Wt/Vol @ 20°C | 1.22 kg/L (10.2 lb/gal) | |
Tukon Hardness | 23 Knoops | |
Viscosity a | 76.5 poise |